Lesintor - 20+Years Industry experience, Professional plastic crusher manufacturers
Most granulators are judged on one number: kilos per hour. A slow edge machine is judged on a different one, and mixing the two up is how plants end up with a unit that is either too slow for the scrap or too aggressive for the part. The LXT-SSC range runs at 24 rpm with no screen at all, on 1.1 to 5.5 kW, in chambers from 290×275 mm to 480×475 mm. That combination is not a de-tuned fast granulator. It is a different cutting regime, and it only makes sense when the material and the location match it.
A conventional granulator turns at 480–650 rpm and relies on impact: blades hit material at speed and shatter it against a screen. A 24 rpm rotor cannot do that. At that speed the knife has to enter the material and shear through it, which means the work comes from torque rather than stored kinetic energy.
Three consequences follow, and all three are practical rather than theoretical.
Heat stays low. Shearing at low speed generates far less frictional heat than repeated impact. For materials that smear or melt at the cut — soft grades, some ABS and PC blends — that is the difference between a clean granule and a chamber full of welded fines.
Noise drops, and so does dust. Impact noise scales with tip speed; at 24 rpm there is very little of it. The same applies to airborne dust, because the machine is not pulverising material that is already small enough.
Throughput is bounded by geometry, not power. With no screen, nothing forces material to stay in the chamber until it is fine. A part either fits the cutting geometry and gets reduced, or it does not. That is the trade: predictable granule shape, but a hard limit on how much the machine will swallow.
A screen does two jobs on a fast granulator: it holds material in the chamber until it is small enough to pass, and it sets a hard ceiling on particle size. Remove it and both jobs move elsewhere.
The ceiling becomes the discharge geometry — the gap between rotor knives and bed knife, and the opening below the rotor. Material leaves when it is physically small enough to fall through, not when it has been hammered through a 6 mm mesh. In practice that means a slow machine produces a flake whose size tracks the blade spacing and the feed orientation, and it produces very few fines, because nothing is held in the chamber to be re-cut.
The holding job disappears entirely, which is the actual advantage. There is no mesh to blind, no holes to peen over, no screen to replace when abrasive filler wears it. On filled or glass-reinforced regrind, screen maintenance is not a marginal cost — it is the item that takes the machine offline. A screenless rotor removes that failure mode.
What it does not remove is the need for a fixed bed knife. The cut quality still depends on the clearance between rotating and fixed knives, and that clearance wears. A slow rotor wears more slowly than a fast one, but it wears.
The range is deliberately narrow, because a slow machine is specified by chamber size rather than by motor size.
| Item | LXT-SSC15P – SSC450 |
|---|---|
| Rotor speed | 24 rpm |
| Motor power | 1.1 – 5.5 kW |
| Cutting chamber | 290×275 – 480×475 mm |
| Screen | None |
| Blade material | SKD-11 |
| Machine weight | 226 – 600 kg |
Read the table from the chamber down, not from the motor up. The chamber opening decides the largest part that can enter, and that is what usually rules a model in or out. Motor size then follows, and it is a modest number by granulator standards — which is the point. A slow rotor does not need a large motor to shear a small part, and a large motor on a slow rotor mostly buys starting torque and tolerance for a dull edge.
Weight matters for a different reason: these machines sit beside a press, often on a mezzanine or a working floor. At 226–600 kg they can be positioned without a structural project, which is not true of a central granulator.
The machine earns its place in a narrow band of applications, and inside that band it is hard to beat.
| Your situation | Fits? | Why |
|---|---|---|
| Sprue and runner from a hard-resin press | Yes | Small, uniform feed; the rotor shears it cleanly at low noise |
| Small technical parts, PC/ABS/PA, rejects at the press | Yes | Low heat keeps the granule colour and avoids smearing |
| Glass-filled material, screen wear is the bottleneck | Yes | No screen to blind or replace |
| Plant with a noise limit near the machine | Yes | Tip speed is a fraction of a fast rotor's |
| Thin film, bags, woven sacks | No | Nothing to shear against; the material wraps the rotor |
| Bulky hollow parts, crates | No | Chamber too small and no grab geometry |
| Mixed plant regrind at high tonnage | No | Throughput is geometry-bound, not power-bound |
The pattern in that table is simple: a slow edge machine is a point-of-generation tool. It is at its best when the scrap is created a metre away and the regrind goes straight back into the same machine's hopper. Move it to a central position and the throughput limit starts to hurt.
Two failure modes show up when a slow granulator is applied outside its band.
The first is feed that cannot be cut. Film, thin sheet and woven material have no section for a shear to bite; they fold, wrap and climb the rotor. Operators then feed harder, the chamber packs, and the machine stalls at 24 rpm with no flywheel energy to recover. There is no screen to remove and no speed to increase — the answer is a different machine, usually one with a film-specific rotor and a much larger throat.
The second is throughput expectation. A buyer comparing kilos per hour across a slow machine and a 15 kW fast granulator will always see the slow one lose. That comparison is meaningless if the slow machine is running beside a press that produces 40 kg of sprue an hour, because neither machine is at its limit. Size the slow unit to the generation rate, not to the plant total.
A slow rotor is forgiving, but not self-maintaining. Two checks carry most of the value.
Blade gap. The clearance between rotating and fixed knives is what turns rotation into a cut. As edges round over, the gap widens and the machine starts nibbling rather than shearing — the symptom is a granule with torn edges and a rise in fines, not a sudden failure. Check the gap on a schedule and adjust before the cut quality drifts.
Chamber condition. With no screen forcing material through, anything that does not fit the discharge geometry stays in the chamber. That makes the chamber itself the maintenance surface: check for build-up of smeared material on the end plates, and check that the discharge opening is clear. A slow machine that suddenly loses output is usually restricted, not dull.
Blade material here is SKD-11, which is the same tool steel used on the faster ranges. It holds an edge well against unfilled resin; against glass-filled material, expect to dress the edge on condition rather than on a calendar.
Does a screenless machine give an uncontrolled particle size?
It gives a wider distribution than a screened machine, not an uncontrolled one. Size follows blade spacing and feed orientation, so a consistent feed produces a consistent flake. What you lose is the hard ceiling a 6 mm screen guarantees.
Can a 24 rpm machine replace a central granulator?
No. It is a beside-the-press tool sized to a generation rate. Central regrind arrives in volumes and shapes that a slow rotor is not built to take.
Is lower noise the main reason to buy one?
It is a real benefit, but the better reason is granule quality and the absence of screen maintenance. Noise usually becomes the deciding factor only on sites with a boundary limit.
Do I still need a screen for fine grinding?
If the specification calls for a maximum particle size below what the rotor geometry produces, yes — and then a screened machine is the correct tool. A slow screenless unit is for regrind that goes back into the same process, not for a graded product.
For plants that want the regrind to go straight back into the press hopper, Lesintor builds the LXT-SSC range from 1.1 kW to 5.5 kW at 24 rpm with SKD-11 blades and no screen, alongside the faster LXT-PC and LXT-MSSC ranges for applications where throughput, not granule shape, is the constraint.